Manufacturing
Quality Trends
Every release in the order it was made, against its specification limits.
Test Torque, peak Texture, visual Appearance vs standard Yield Peak temperature Fusion time Moisture Colour, initial ΔE Metal content Bulk density Sieve residue 75 µm Assay Viscosity 25°C Melting point Free fatty acid Tin content Heavy metals
Grade
Every grade
ACE-CAS10 ACE-CAS20 ACE-CAS30-FG ACE-CAS40-C ACE-LIS10 ACE-MGS10 ACE-MGS20-PH ACE-ZNS10 ACE-ZNS20-C ACEFEED-CA20 ACEGUARD-HT8 INT-CAST70 INT-CZB40 SAK-BZL40 SAK-CZB65 SAK-CZC60 SAK-CZC70 SAK-CZG90 SAK-CZH80 SAK-CZM15 SAK-CZM18 SAK-CZP30 SAK-CZP35 SAK-CZP40 SAK-CZS10 SAK-CZW50 SAK-ORP22 SAK-OTM70
Releases plotted
21
SAK-CZP 30 · Ca/Zn one pack, pressure pipe
Average yield
99.43%
Specification 97.50 to 100.00% · target 99.40%
+0.03 against target
Outside specification
0
Every release inside its limits
Clean run
Process capability, Cpk
0.96
Spread is wide against the limits
σ 0.20%
Yield by batch, in the order it was made
Red bands are the specification limits, the dashed line is target.
Inside spec Near a limit Out of spec
Worth a look
Releases outside a limit or close to one, newest first.
| Batch | Made | Yield | On the job before | Where |
|---|---|---|---|---|
| B26-0259 SAK-CZP30 | 14 May 2026 | 99.79% Near a limit | +0.29 | WO-2026-0259 BL-01 · Malcolm Rees |
The biggest movement in the run
The largest change from one job to the next.