Specifications 7 plans · 4 written tighter
July 2026 close · posted live Mon 3 Aug 2026

Quality

Specifications

What each product is tested for, and the tolerance on every test.

Release plans

7

One per product class, plus incoming goods

Tests defined

49

Across every plan

Grades held tighter

3

Narrower than the plan they release under

Customer specifications

2

Written into a supply agreement

Where the tolerance differs

Every specification written tighter than the plan, and what it was tightened from.

Reference Applies to Test Plan says Held to
SA-CZP30-A
since 30 Jun 2025
Pressure pipe. The grade is held tighter than the one-pack plan on colour and on initial fusion.
SAK-CZP30
SAK-CZP 30 · Ca/Zn one pack, pressure pipe
Every customer
Colour, initial ΔE 0.00 to 3.50 ΔE 0.00 to 2.40 ΔE
Fusion time 54.0 s ±3% 54.0 s ±2%
IPX-CZP30-04
since 16 Feb 2026
Iplex supply agreement, clause 7. Tighter again on moisture and colour, and a bulk density window they extrude to.
SAK-CZP30
SAK-CZP 30 · Ca/Zn one pack, pressure pipe
Iplex Pipelines Australia Pty Ltd
Moisture 0.00 to 1.50 % 0.00 to 0.90 %
Colour, initial ΔE 0.00 to 3.50 ΔE 0.00 to 1.80 ΔE
Bulk density 260 to 400 g/L 300 to 350 g/L
VDX-CZP40-02
since 04 Nov 2025
Vinidex hold the fusion time to plus or minus two per cent on sewer and drainage.
SAK-CZP40
SAK-CZP 40 · Ca/Zn one pack, sewer & drainage pipe
Vinidex Pty Ltd
Fusion time 54.0 s ±3% 54.0 s ±2%
SA-CAS30-FG
since 01 Sep 2024
Food contact. Heavy metals half the plan limit, and the assay window narrowed.
ACE-CAS30-FG
ACE-CAS 30 FG · calcium stearate, food & kosher approved
Every customer
Heavy metals 0.0 to 10.0 ppm 0.0 to 5.0 ppm
Assay 98.00 to 101.50 % 98.50 to 101.00 %

What the certificate looks like

Four documents off one set of results. A variant chooses what to print, never what was measured.

Document Accounts Also prints Because
General certificate
COA-GENERAL
26 The release tests only What most accounts receive. Release tests, result against specification, and the batch it came from.
Pipe extrusion variant
COA-PIPE
5 Black specks, Pour density Pipe extruders read speck count off the plaque because it shows on the finished pipe. Reported, not released on.
Food contact variant
COA-FOOD
5 Loss on drying, Vegetable origin Food and personal care accounts. Adds the origin declaration and loss on drying.
Export and intercompany variant
COA-EXPORT
12 Loss on drying Adds country of origin, which customs at the far end asks for.

One-pack stabiliser release

QP-ONEPACK

Run at the end of manufacture, before the goods can be receipted into finished goods.

45 grades release under it , 3 of them with something written tighter

Test Target Tolerance
Yield 99.40 % 97.50 to 100.00 %
Peak temperature 135.0 °C 128.0 to 142.0 °C
Fusion time 54.0 s ±3%
Torque, peak 42.0 Nm ±3%
Colour, initial ΔE 1.60 ΔE 0.00 to 3.50 ΔE
Bulk density 320 g/L 260 to 400 g/L
Moisture 0.60 % 0.00 to 1.50 %
Texture, visual Conforms Against the retained standard

Grades

SAK-CZP30, SAK-CZP35, SAK-CZP40, SAK-CZF20, SAK-CZF25, SAK-CZW50, SAK-CZW55, SAK-CZC60, SAK-CZC70, SAK-CZC75 and 35 more

Metallic stearate release

QP-STEARATE

Precipitated and fused stearates. Metal content and sieve residue decide the grade.

15 grades release under it

Test Target Tolerance
Yield 99.40 % 97.50 to 100.00 %
Peak temperature 135.0 °C 128.0 to 142.0 °C
Metal content 6.80 % 6.20 to 7.40 %
Moisture 0.60 % 0.00 to 1.50 %
Bulk density 320 g/L 260 to 400 g/L
Sieve residue 75 µm 0.10 % 0.00 to 0.50 %
Melting point 155.0 °C 145.0 to 165.0 °C
Free fatty acid 0.50 % 0.00 to 1.20 %

Grades

ACE-CAS10, ACE-CAS20, ACE-ZNS10, ACE-ZNS20-C, ACE-MGS10, ACE-BAS10, ACE-NAS10, ACE-LIS10, ACE-CAS40-C, ACE-CAS50-M and 5 more

Food-contact & kosher release

QP-FOODCONTACT

Adds heavy metals and appearance against the retained standard. Vegetable origin declared BSE free.

6 grades release under it , 1 of them with something written tighter

Test Target Tolerance
Yield 99.40 % 97.50 to 100.00 %
Peak temperature 135.0 °C 128.0 to 142.0 °C
Metal content 6.80 % 6.20 to 7.40 %
Moisture 0.60 % 0.00 to 1.50 %
Heavy metals 2.0 ppm 0.0 to 10.0 ppm
Assay 99.60 % 98.00 to 101.50 %
Appearance vs standard Conforms Against the retained standard
Sieve residue 75 µm 0.10 % 0.00 to 0.50 %

Grades

SAK-CZM15, SAK-CZL18, ACE-CAS30-FG, ACE-ZNS30-FG, ACEFEED-CA20, SAK-CZB65

Pharmacopoeial release

QP-PHARMA

Full monograph assay with retained sample. Certificate of analysis issued with every despatch.

3 grades release under it

Test Target Tolerance
Yield 99.40 % 97.50 to 100.00 %
Assay 99.60 % 98.00 to 101.50 %
Heavy metals 2.0 ppm 0.0 to 10.0 ppm
Moisture 0.60 % 0.00 to 1.50 %
Metal content 6.80 % 6.20 to 7.40 %
Appearance vs standard Conforms Against the retained standard
Sieve residue 75 µm 0.10 % 0.00 to 0.50 %

Grades

ACE-MGS20-PH, ACEPURE-SC5, SAK-CZM18

Liquid mixed-metal release

QP-LIQUID

Liquid Ba/Zn and Ca/Zn grades, viscosity and colour on the drum.

2 grades release under it

Test Target Tolerance
Yield 99.40 % 97.50 to 100.00 %
Peak temperature 135.0 °C 128.0 to 142.0 °C
Fusion time 54.0 s ±3%
Torque, peak 42.0 Nm ±3%
Viscosity 25°C 250 mPa·s 180 to 340 mPa·s
Colour, initial ΔE 1.60 ΔE 0.00 to 3.50 ΔE
Metal content 6.80 % 6.20 to 7.40 %
Appearance vs standard Conforms Against the retained standard

Grades

SAK-BZL40, SAK-BZL45

Organotin release

QP-TIN

Mercaptide grades. Tin assay against specification before drumming.

4 grades release under it

Test Target Tolerance
Yield 99.40 % 97.50 to 100.00 %
Peak temperature 135.0 °C 128.0 to 142.0 °C
Torque, peak 42.0 Nm ±3%
Tin content 18.40 % 17.50 to 19.50 %
Viscosity 25°C 250 mPa·s 180 to 340 mPa·s
Colour, initial ΔE 1.60 ΔE 0.00 to 3.50 ΔE
Appearance vs standard Conforms Against the retained standard

Grades

SAK-OTM70, SAK-OTO80, SAK-OTB60, SAK-OTS90

Incoming goods inspection

QP-INCOMING

Raw materials and traded goods: certificate check, identity and appearance. Fails move to Quarantine.

0 grades release under it

Test Target Tolerance
Assay 99.60 % 98.00 to 101.50 %
Moisture 0.60 % 0.00 to 1.50 %
Appearance vs standard Conforms Against the retained standard

The window is computed from the target and the tolerance, never typed alongside it.